This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2017, 8, 906–914, doi:10.3762/bjnano.8.92
Figure 1: A schematic of the foaming process showing the critical steps to obtain a sample with a controlled ...
Figure 2: SEM images of the cross section with a gradient of pores before and after indentation. (a) The orig...
Figure 3: Pore distribution for the indentation columns 1 (top) and 5 (bottom). All presented data fit to a l...
Figure 4: Relation between pore wall thickness, pore diameter, and pore fraction in micro-to-nanocellular PMM...
Figure 5: Storage and loss moduli (a) and loss factor (b) measured on the 5 × 4 arrays with flat-punch indent...
Figure 6: Change of the number- (Mn) and mass- (Mw) average of the molar mass in PMMA before and after foamin...